OBSH vs AC Blowing Agent for Microcellular Rubber: Shoe Soles, Seals & Density Control

Oct 28, 2026 Beihua

A side-by-side look at OBSH and azodicarbonamide (AC) to help compounders pick the right foaming agent for microcellular soles and seals.

The Choice in a Nutshell

OBSH gives fine, uniform cells at lower temperature with no ammonia odor; AC delivers higher gas volume at higher temperature and is more economical.

OBSH-75 Masterbatch

75% active OBSH in a polymer carrier. Dosage 1–3 phr. Ideal for EPDM/NBR microcellular soles and seals where low odor and cell control matter.

AC Blowing Agent

Dosage 2–5 phr. Higher decomposition temperature and gas yield suit thicker, high-expansion parts but may need an activator and odor control.

Decision Checklist

Match decomposition temperature to cure profile, target density and odor limits. Masterbatch form eliminates dust for both agents.

TDS / Technical Data Sheet

Products OBSH-75 / AC Blowing Agent
OBSH active content 75% min.
AC active content 95–99% (granular grade)
Carrier (OBSH) EPDM / SBR polymer
Appearance White to off-white granules
Decomposition temperature OBSH 155–165°C / AC 200–210°C
Gas volume (mL/g) OBSH ~125 / AC ~220
Shelf life 12 months

SDS Highlights

Thermal decomposition releases gases – avoid confined heating and provide ventilation. AC may release traces of formaldehyde; use activated carbon/odor scavenger. Wear gloves and eye protection.

COA Sample

Batch No. OBS25-1011
OBSH content 75.4%
Decomposition temp 160°C
Gas volume 126 mL/g
Appearance Conforms
Result PASS

Product Information

Packaging 25 kg paper bag; 1,000 kg per pallet (OBSH and AC packed separately)
MOQ 500 kg (approx. 20 bags)
Shipping port Shanghai Port / Ningbo Port, China
OBSH blowing agent AC blowing agent microcellular rubber foaming cell size control

+8613706519013